Mg–1Zn–1Ca alloy for biomedical applications. Influence of the secondary phases on the mechanical and corrosion behaviour

dc.contributor.authorPulido-González, Nuria
dc.contributor.authorTorres, Belén
dc.contributor.authorGarcía-Rodríguez, Sonia
dc.contributor.authorRodrigo, Pilar
dc.contributor.authorBonache, Victoria
dc.contributor.authorHidalgo-Manrique, Paloma
dc.contributor.authorMohedano, Marta
dc.contributor.authorRams, Joaquín
dc.date.accessioned2024-04-09T08:06:21Z
dc.date.available2024-04-09T08:06:21Z
dc.date.issued2020-08-05
dc.identifier.citationN. Pulido-González, B. Torres, S. García-Rodríguez, P. Rodrigo, V. Bonache, P. Hidalgo-Manrique, M. Mohedano, J. Rams, Mg–1Zn–1Ca alloy for biomedical applications. Influence of the secondary phases on the mechanical and corrosion behaviour, Journal of Alloys and Compounds, Volume 831, 2020, 154735, ISSN 0925-8388, https://doi.org/10.1016/j.jallcom.2020.154735es
dc.identifier.issn0925-8388
dc.identifier.urihttps://hdl.handle.net/10115/32157
dc.description.abstractAn as-cast Mg–1Zn–1Ca alloy has been soundly characterized to be used as a biodegradable material in biomedical applications. Ca and Zn additions have a great influence in the microstructure, mechanical properties and corrosion behaviour of Mg alloys. SEM examinations revealed that most of the Ca and Zn atoms form Mg2Ca and Ca2Mg6Zn3 precipitates, which distribute preferentially along the grain boundaries forming a continuous network of secondary phases. The results of nanoindentation tests show differences in hardness and elastic modulus between the α-Mg matrix and the secondary phases. The results of three-point bending tests shows that cracks propagate following the network formed by the intermetallic compounds at the grain boundaries (GBs). The evolved hydrogen after immersion in Hank’s solution of the alloy has been also estimated, showing a change in the corrosion mechanism after 160 h. The intermetallic compounds act as a barrier against corrosion, so that it progresses through the α-Mg matrix phase.es
dc.language.isoenges
dc.publisherElsevieres
dc.rightsAttribution-NonCommercial-NoDerivatives 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.subjectMg-Zn-Ca alloys; Biomaterials; Biodegradable implants; Three-point bending test; Nanoindentation; Corrosion behavioures
dc.titleMg–1Zn–1Ca alloy for biomedical applications. Influence of the secondary phases on the mechanical and corrosion behavioures
dc.typeinfo:eu-repo/semantics/articlees
dc.identifier.doi10.1016/j.jallcom.2020.154735es
dc.rights.accessRightsinfo:eu-repo/semantics/openAccesses


Fichier(s) constituant ce document

Ce document figure dans la(les) collection(s) suivante(s)

Afficher la notice abrégée

Attribution-NonCommercial-NoDerivatives 4.0 InternacionalExcepté là où spécifié autrement, la license de ce document est décrite en tant que Attribution-NonCommercial-NoDerivatives 4.0 Internacional