Effect of temperature on the fracture behaviour of polyamide 12 and glass-filled polyamide 12 processed by selective laser sintering 203
dc.contributor.author | Cano, Alberto Jesús | |
dc.contributor.author | Salazar, López | |
dc.contributor.author | Rodríguez, Jesús | |
dc.date.accessioned | 2024-01-08T09:19:42Z | |
dc.date.available | 2024-01-08T09:19:42Z | |
dc.date.issued | 2018-07-26 | |
dc.description | Este trabajo ha sido financiado por el Ministerio de Economía y Competitividad de España a través del proyecto con referencia DPI2016-80389-C2-1-R. | es |
dc.description.abstract | The influence of the orientation and of the temperature on the mechanical properties of the polyamide 12 (PA12) and the polyamide 12 reinforced with glass beads processed via Selective Laser Sintering was analyzed. Tensile and fracture tests were performed at −50 °C, 23 °C and 50 °C with applied load perpendicular and parallel to the layered structure. The fracture resistance of PA12 was higher than that of the composite due to the poor adhesion of the glass beads to the matrix. The fracture behavior of the composite was unaffected by the temperature and the orientation. JIC values of PA12 were similar at −50 °C and at 23 °C and much lower than at 50 °C. The anisotropy was relevant during the stable crack growth. | es |
dc.identifier.citation | Cano, A.J., Salazar, A., Rodríguez, J. Effect of temperature on the fracture behaviour of polyamide 12 and glass-filled polyamide 12 processed by selective laser sintering. Eng Fract Mech 2018; 203: 66-80. DOI:10.1016/j.engfracmech.2018.07.035 | es |
dc.identifier.doi | 10.1016/j.engfracmech.2018.07.035 | es |
dc.identifier.issn | 0013-7944 | |
dc.identifier.uri | https://hdl.handle.net/10115/28211 | |
dc.language.iso | eng | es |
dc.publisher | PERGAMON-ELSEVIER SCIENCE LTD | es |
dc.rights | Attribution-NonCommercial-NoDerivatives 4.0 Internacional | * |
dc.rights.accessRights | info:eu-repo/semantics/embargoedAccess | es |
dc.rights.uri | http://creativecommons.org/licenses/by-nc-nd/4.0/ | * |
dc.subject | Selective laser sintering | es |
dc.subject | Polyamide 12 | es |
dc.subject | Fracture toughness | es |
dc.title | Effect of temperature on the fracture behaviour of polyamide 12 and glass-filled polyamide 12 processed by selective laser sintering 203 | es |
dc.type | info:eu-repo/semantics/article | es |
Archivos
Bloque original
1 - 1 de 1
No hay miniatura disponible
- Nombre:
- Eng Fract Mech 203 2018.pdf
- Tamaño:
- 5.37 MB
- Formato:
- Adobe Portable Document Format
- Descripción: