Thiol group functionalization of mesoporous SiO2 SBA-15 using supercritical CO2

dc.contributor.authorTenorio, Maria Jose
dc.contributor.authorMorere, Jacobo
dc.contributor.authorCarnerero, Cyntia
dc.contributor.authorTorralvo, Maria Jose
dc.contributor.authorPando, Concepcion
dc.contributor.authorCabañas, Albertina
dc.date.accessioned2024-01-23T07:48:42Z
dc.date.available2024-01-23T07:48:42Z
dc.date.issued2018
dc.description.abstractChemical modification of mesoporous SiO2 SBA-15 with thiol groups was performed using mercaptopropyltrimethoxysilane (MPTMS) dissolved in supercritical CO2 (scCO2). Thiol groups serve as adsorbents for the selective removal of contaminant metal cations and in catalysis. Functionalization was carried out in scCO2 at temperatures ranging from 40 to 150 C and pressures from 15.0 to 29.0 MPa. For comparison purposes, the reaction was also performed in toluene at 80 and 110 C. As opposed to toluene, scCO2 is considered a green solvent. Grafting of the thiol groups was confirmed by FTIR spectroscopy, thermogravimetric analysis (TGA) and elemental analysis. Grafting density and surface coverage of the materials modified using scCO2 increased with temperature, CO2 density, time and stirring and varied from 1.3 to 4.4 mmol/ g and from 1.3 to 4.0 molecules/ nm, respectively. On the other hand, surface area and pore size decreased as grafting density increased. At temperatures of 80 C or higher, the pore size remained constant, suggesting the formation of a compact monolayer. Modification at higher temperatures led to larger grafting densities but very low surface areas. Assuming total hydrolysis and condensation of the precursor, the optimum grafting density and surface coverage of 2.3 mmol/ g and 2.4 molecules/ nm, respectively, were obtained in scCO2 at 80 C and 25.0 MPa for 4 h. Grafting densities of the samples prepared in toluene were by far much lower than those obtained using scCO2 at lower temperatures and shorter times, which demonstrates the advantages of CO2 as a green functionalization medium.es
dc.identifier.citationMicroporous and Mesoporous Materials 256 (2018) 147e154es
dc.identifier.doi10.1016/j.micromeso.2017.07.056es
dc.identifier.issn1387-1811
dc.identifier.urihttps://hdl.handle.net/10115/28671
dc.language.isoenges
dc.publisherElsevieres
dc.rightsAttribution-NonCommercial-NoDerivatives 4.0 Internacional*
dc.rights.accessRightsinfo:eu-repo/semantics/restrictedAccesses
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.subjectSurface modificationes
dc.subjectSupercritical fluidses
dc.subjectSustainable chemistryes
dc.subjectMesoporouses
dc.subjectSiO2 SBA-15es
dc.titleThiol group functionalization of mesoporous SiO2 SBA-15 using supercritical CO2es
dc.typeinfo:eu-repo/semantics/articlees

Archivos

Bloque original

Mostrando 1 - 1 de 1
No hay miniatura disponible
Nombre:
Aportación_2_Tenorio_MicroporousMesoporousMaterials_2018.pdf
Tamaño:
1.11 MB
Formato:
Adobe Portable Document Format
Descripción:
Articulo publicado

Bloque de licencias

Mostrando 1 - 1 de 1
No hay miniatura disponible
Nombre:
license.txt
Tamaño:
2.67 KB
Formato:
Item-specific license agreed upon to submission
Descripción: